Siding - Conformance
Typical Physical Properties
TestStandard MethodUnit of MeasureResult
IZOD impact (23°C/73°F)ASTM D-256ft-lb/in2.4
Tensile strengthASTM D-638Psi>6000
Modulus of elasticityASTM D-638Psi>365,000
Deflection temperature under load @ 264 Psi ASTM D-648°F170
Coefficient of linear expansion ASTM E-831105 in/in/°F3.07
Chemical resistanceASTM D-543Excellent
Cell classificationASTM D-1784 Class #1334434
Compound classASTM D-3679Class #2
Siding/Extrudate Typical Physical Properties
TestStandard MethodUnit of MeasureResult
Impact resistance (23°C/73°F)ASTM D-4226in-lb/mil2.75
Impact resistance (0°C/32°F) ASTM D-4226in-lb/mil1.90
Low temperature flexibility CAN/CGSB41 - 24-95% passed>80
Shrinkage/reversion ASTM D-3679-95%<3.0
Surface distortion (oil can)ASTM D-3679-95°F>150
Nominal thickness CAN/CGSB41 - 24-95 mm1.17
Wall thicknessASTM D-3679-95inch0.040
Fire Characteristics
TestStandard MethodResult
Flame spread index
Fuel contribution
Smoke developed index
ASTM E84, UBC 42-118
0
510.2
Self-ignition temperature, °F ASTM D-1929, UBC 52-3810
Smoke density rating (%)
Maximum smoke density (%)
Visibility of exit sign
ASTM D-2843, UBC 52-242.1
56.0
Good
Total burn time, seconds
Extent of burning, mm
Fire resistance rating
ASTM D-635
ASTM D-635
ASTM E-119
<5
<5
1 hour